Growth of High-Quality Oxides on The Inner Surface of ECMO Circuit by Atomic Layer Deposition to Reduce Thrombus Formation
试验速览
- 阶段
- 不适用
- 状态
- 已完成
- 入组人数
- 4
- 试验地点
- 1
- 主要终点
- Protein content or configuration changed
研究概览
简要总结
This study evaluate thermal ALD (T-ALD) and plasma-enhance ALD (PE-ALD) processes modified cardiopulmonary bypass (CPB) tubing to investigate anticoagulation properties.
详细描述
ECMO is a technique which is currently being used worldwide for providing life support for patients experiencing both pulmonary and cardiac failure. Though ECMO can effectively rescue life at the initial scene, being invasive, complex, resource intensive, and serious related complications developing on the following days of ECMO support have greatly restricted it use. The major causes of ECMO-related mortality and morbidity are serious coagulopathy, either bleeding (7-34%) or thrombosis (8-17%). Contact of high extracorporeal blood flow and the large artificial surfaces plays a critical role leading to the subsequent coagulopathy. Systemic heparin and heparin-bonded circuits is usually used to reduce thrombus. However, non-urgent invasive procedures should be avoided or minimized during that support and regular clinical monitoring to guide the adjustment of optimal dosage is mandatory making the clinical care intensive. Whereas the pharmacological interventions may bring the risk of critical imbalance between hemostasis and thrombosis, efforts to modify the ECMO system focusing on improvement of biocompatibility seem a fundamental way particularly regarding the extended periods of ECMO use. ZrO2 and Al2O3 are more excellent biocompatible and hemocompatible materials compared with PVC (polyvinylchloride) which is the current material of ECMO circuit. Despite the broad applications of ZrO2 and Al2O3 in artificial implants, traditional thin-film coating techniques are unable to deposit these hemocompatible oxides on the inner surface of the PVC tubing in ECMO circuit. In this subproject, the investigators will apply a new technique of atomic layer deposition (ALD) to coat biocompatible and hemocompatible ZrO2/Al2O3 nanolaminate thin films on the inner surface of ECMO tubing to suppress the device-induced coagulopathy. ALD is a thin-film deposition technique for preparing high-quality oxides with atomic-layer accuracy. It offers many benefits including accurate thickness control, excellent conformality, high uniformity, low defect density, good reproducibility, and low deposition temperature. These characteristics clearly accounts for the feasibility to deposit high-quality hemocompatible oxide thin films on the whole surface of complex 3-D structures, such as the inner surface of ECMO tubing, using the ALD technique. The newly-prepared ECMO circuit will then undergo in vitro tests and animal study to carefully examine the safety and effectiveness of improvement of hemocompatibility.
研究设计
- 研究类型
- Interventional
- 分配方式
- Na
- 干预模型
- Single Group
- 主要目的
- Supportive Care
- 盲法
- None
入排标准
- 年龄范围
- 20 Years 至 —(Adult, Older Adult)
- 性别
- All
- 接受健康志愿者
- 是
入选标准
- •Weighing more than 50 kg
排除标准
- •Pregnancy
- •Chewing betel nut
- •History of any blood or cancer
- •Taking anticoagulants
研究组 & 干预措施
ECMO tube
干预措施: ECMO (Other)
结局指标
主要结局
Protein content or configuration changed
时间窗: Within 3 days after blood drawed
Use ELISA to measuring the content or configuration of a protein when blood contact material, such as human serum albumin and human plasma fibrinogen etc.