Y-TZP and In-mouth Low Thermal Degradation: A Prospective Clinical Study
- Conditions
- Zirconia Monolithic Dental Restorations: In-mouth Behaviour, LTD and Wear
- Interventions
- Device: Lava plus (3M) crowns and bridges
- Registration Number
- NCT02150226
- Lead Sponsor
- University of Liege
- Brief Summary
The objective of this work is to study in-mouth aging and LTD of monolithic zirconia restorations. Microstructural changes characteristic of LTD processes, wear, and clinical behaviour following standard parameters will be evaluated. Notably Raman spectroscopy and 3D laser surface analysis will be used, directly on the restorations, which will be removed at regular intervals.The working hypothesis is that LTD process is very slow at the scale at the lifespan of dental prostheses.
- Detailed Description
Not available
Recruitment & Eligibility
- Status
- UNKNOWN
- Sex
- All
- Target Recruitment
- 101
- Full zirconia crowns in the posterior region (molar/premolar)
- On teeth or implants
- Single unit restorations cemented on natural teeth and implants (including screw-retained restorations if possible, but no internal connections)
- Multi-unit restorations on implants
- If nightguard: to be performed on the antagonist
- Patients with removable prosthesis as an antagonist
Study & Design
- Study Type
- INTERVENTIONAL
- Study Design
- SINGLE_GROUP
- Arm && Interventions
Group Intervention Description Experimental: Zirconia monolithic crowns and bridges Lava plus (3M) crowns and bridges Evaluation of Lava Plus zirconia dental crowns and bridges
- Primary Outcome Measures
Name Time Method in-mouth LTD of monolithic zirconia restorations on natural teeth and implants up to 5 years
- Secondary Outcome Measures
Name Time Method
Trial Locations
- Locations (1)
Institute of Dentistry University of Liege
🇧🇪Liege, Belgium